Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1590 MPa | 230000 psi | Transverse Rupture |
Pacific Sintered Materials FN-253-T(HT) 4600 Powdered Metal High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FL-4605-140HTAll information provided by Pacific Sintered Metals. |
|||
Flexural Strength | 1590 MPa | 230000 psi | Transverse Rupture |
PSM Industries Pacific Sintered Metals 4600 F-253-T(HT) Powdered Metal High performance material with high strength and wear resistance after heat treatment Equivalent MPIF Specification: FL-4605-140HTInformation Provided by Pacific Sintered Metals, a division of PSM .. |