Mechanical Properties Metric English Comments
Flexural Strength 103.01 MPa
14940 psi
ASTM D790
E-Polymers TEKAPPO® JF1 Un-Reinforced Flame Retardant M-PPO
Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a..
Flexural Strength 103.01 MPa
14940 psi
ASTM D790
E-Polymers TEKASTER® F101FR Un-Reinforced Flame Retardant PBT
Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe..
Flexural Strength 103.01 MPa
14940 psi
ASTM D790
E-Polymers TEKAPPO® JF101 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO
Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a..