Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 103.01 MPa | 14940 psi | ASTM D790 |
E-Polymers TEKAPPO® JF1 Un-Reinforced Flame Retardant M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Flexural Strength | 103.01 MPa | 14940 psi | ASTM D790 |
E-Polymers TEKASTER® F101FR Un-Reinforced Flame Retardant PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Flexural Strength | 103.01 MPa | 14940 psi | ASTM D790 |
E-Polymers TEKAPPO® JF101 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |