Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 101.7 MPa | 14750 psi | ASTM D790 |
PolyOne Edgetek® ATH-30GF/000 Acetal-Homopolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |