Polymer Property : Flexural Strength = 101.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 101.7 MPa
14750 psi
ASTM D790
PolyOne Edgetek® ATH-30GF/000 Acetal-Homopolymer, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.