Mechanical Properties Metric English Comments
Flexural Strength 75.0 - 79.0 MPa
10900 - 11500 psi
ASTM D790
3D Systems Accura® Xtreme White 200 Plastic
Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl..