Material Notes:
Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembliesUsed for master patterns for vacuum castingAll information provided by 3D Systems.
Physical Properties Metric English Comments
Density 1.12 g/cc

@Temperature 25.0 °C
0.0405 lb/in³

@Temperature 77.0 °F
Liquid
1.18 g/cc

@Temperature 25.0 °C
0.0426 lb/in³

@Temperature 77.0 °F
Solid
Viscosity 650 - 750 cP

@Temperature 30.0 °C
650 - 750 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 78 - 80
78 - 80
Tensile Strength 45.0 - 50.0 MPa
6530 - 7250 psi
ASTM D638
Elongation at Break 7 - 20 %
7 - 20 %
ASTM D638
Tensile Modulus 2.30 - 2.60 GPa
334 - 377 ksi
ASTM D638
Flexural Strength 75.0 - 79.0 MPa
10900 - 11500 psi
ASTM D790
Flexural Modulus 1.52 - 2.07 GPa
220 - 300 ksi
ASTM D790
Izod Impact, Notched 0.550 - 0.600 J/cm
1.03 - 1.12 ft-lb/in
ASTM D256
Penetration 4.6
4.6
mils penetration depth
Thermal Properties Metric English Comments
CTE, linear 95.0 µm/m-°C

@Temperature 30.0 - 50.0 °C
52.8 µin/in-°F

@Temperature 86.0 - 122 °F
180 µm/m-°C

@Temperature 70.0 - 140 °C
100 µin/in-°F

@Temperature 158 - 284 °F
Deflection Temperature at 0.46 MPa (66 psi) 47.0 °C
117 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C
108 °F
ASTM D648
Glass Transition Temp, Tg 52.0 °C
126 °F
DMA, E"
Descriptive Properties Value Comments
Appearance White
Critical Exposure (mJ/cm²) 8.3