Mechanical Properties Metric English Comments
Flexural Strength 1150 MPa
167000 psi
0° stress angle
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Unidirectional
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..
Flexural Strength 1150 MPa
167000 psi
ASTM D790
Dow Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Strip
FULCRUM Thermoplastic Composite Technology is specifically designed for the fabrication of continuous fiber composites that have greater flexibility in post-processing operations as well as higher t..