Dow Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Strip

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
Manufacturer Dow Chemical
Trade Name Fulcrum™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Strip.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FULCRUM Thermoplastic Composite Technology is specifically designed for the fabrication of continuous fiber composites that have greater flexibility in post-processing operations as well as higher toughness and faster production rates than traditional composite materials. The technology, using ISOPLAST® Engineering Thermoplastic Polyurethane (ETPU), allows production of hollow as well as solid elongated profiles using pultrusion techniques.Information provided by Dow Chemical.
Physical Properties Metric English Comments
Density 1.91 g/cc
0.0690 lb/in³
ASTM D792
Filler Content 76 %
76 %
Glass
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1000 MPa
145000 psi
ASTM D3039
Elongation at Break 2.2 %
2.2 %
In Tension; ASTM D3039
Modulus of Elasticity 45.0 GPa
6530 ksi
ASTM D3039
Flexural Strength 120 MPa
17400 psi
Transverse; ASTM D790
1150 MPa
167000 psi
ASTM D790
Flexural Modulus 6.00 GPa
870 ksi
Transverse; ASTM D790
45.0 GPa
6530 ksi
ASTM D790
Izod Impact, Notched 42.0 J/cm
78.7 ft-lb/in
ASTM D256
Izod Impact, Unnotched 59.0 J/cm
111 ft-lb/in
3 strips glued together; ASTM D4812
Impact Test 30.0 J
22.1 ft-lb
Instrumented Impact; 20 mm width sample; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 9.00 µm/m-°C

@Temperature 20.0 °C
5.00 µin/in-°F

@Temperature 68.0 °F
ASTM D696
CTE, linear, Transverse to Flow 5.20 µm/m-°C

@Temperature 20.0 °C
2.89 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 80.0 °C
176 °F
Heat Deflection Temp; Load not specified
Glass Transition Temp, Tg 90.0 °C
194 °F
G" in DMS