Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 113.8 MPa | 16500 psi | |
Shinil Chemical SHINSTRA PC/PET TES Structural Polymer Car Spoiler SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog.. |