Mechanical Properties Metric English Comments
Flexural Strength 724 MPa
105000 psi
Rigidty. Elastic bending fatigue, Transverse
CLAL-MSX NICLAFOR® 1000 TH1 Quenched/Precipitation Heat Treated, Rolled Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Flexural Strength 724 MPa
105000 psi
Anderman Ceramics EZM 96 Zirconia, 96.5%, Magnesia-Stabilized
Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes.
Copyright © lookpolymers.com All Rights Reserved