Mechanical Properties Metric English Comments
Flexural Strength 103.45 MPa
15004 psi
ASTM D790
Lucent Polymers 6-01 Nylon 6, General Purpose, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizedTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.