Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 60.0 - 70.0 MPa | 8700 - 10200 psi | ASTM D790-03 |
Proto3000 Objet Digital Materials™ DM_8210 Rigid Opaque Prototyping Polymer Primary material: VeroBlueSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the .. |
|||
Flexural Strength | 60.0 - 70.0 MPa | 8700 - 10200 psi | ASTM D790-03 |
Proto3000 Objet VeroBlue FullCure840 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Flexural Strength | 40.0 - 70.0 MPa | 5800 - 10200 psi | Longitudinal |
Quadrant Plastic Composites MultiQ® Concrete Thermoplastic Panel Composite MultiQ is a product line of thermoplastic composites in panel form whose specific properties make them particularly suitable as an environmental alternative to plywood in outdoor applications. Howev.. |
|||
Flexural Strength | 60.0 - 70.0 MPa | 8700 - 10200 psi | Compression; ISO 178 |
Raschig Group 4552 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi.. |
|||
Flexural Strength | 50.0 - 70.0 MPa | 7250 - 10200 psi | Compression; ISO 178 |
Raschig Group DECAL® 937 Phenolic Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W.. |
|||
Flexural Strength | 50.0 - 70.0 MPa | 7250 - 10200 psi | |
GrafTech GRAFCELL® FFP-100 SERIES Flow Field Plate Graphite Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid.. |
|||
Flexural Strength | 50.0 - 70.0 MPa | 7250 - 10200 psi | |
GrafTech GRAFCELL® FFP-200 SERIES Flow Field Plate Graphite Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid.. |
|||
Flexural Strength | 50.0 - 70.0 MPa | 7250 - 10200 psi | |
GrafTech GRAFCELL® FFP-300 SERIES Flow Field Plate Graphite Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid.. |
|||
Flexural Strength | 66.7 - 70.5 MPa | 9670 - 10200 psi | ASTM D790M |
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC -2 DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons.. |