Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 102.04 MPa | 14800 psi | |
Abatron AboCast 8-2/Abocure 8-2 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 100 g (3.5 oz.): 265 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adh.. |