Material Notes:
2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 100 g (3.5 oz.): 265 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adhesive, and coating.
Physical Properties Metric English Comments
Water Absorption 0.21 %
0.21 %
in 24 hours.
Viscosity Measurement 1600
1600
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
Tensile Strength, Ultimate 62.05 MPa
9000 psi
Elongation at Break 4.0 %
4.0 %
Flexural Strength 102.04 MPa
14800 psi
Izod Impact, Notched 0.272 J/cm
0.510 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 62.0 °C
144 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity 5.00e+11 ohm-cm

@Temperature 93.3 °C
5.00e+11 ohm-cm

@Temperature 200 °F
1.00e+13 ohm-cm

@Temperature 65.6 °C
1.00e+13 ohm-cm

@Temperature 150 °F
3.00e+15 ohm-cm

@Temperature 25.0 °C
3.00e+15 ohm-cm

@Temperature 77.0 °F
Dielectric Constant 3.41

@Frequency 1e+6 Hz
3.41

@Frequency 1e+6 Hz
Dissipation Factor 0.012

@Frequency 1e+6 Hz
0.012

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Curing time: 3 weeks