Mechanical Properties Metric English Comments
Flexural Strength 0.460 MPa
66.7 psi
As received, Parallel to Thickness
Zircar Ceramics ASQ Castertip
14 pcf density refractory ceramic fiber "soft tip". Alumina bonding of shot free fiber results in extreme performance in manufacture of the finest grades of medical, food and packaging foils. Inform..