Mechanical Properties Metric English Comments
Flexural Strength 0.369 MPa
53.5 psi
48 hour silo aging time, 20 kg/m^3
Jackon JACKOCELL® R411 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionThe unique design of polystyrene chains and additive chemistry in the Jackocell® R411 gives pre-expanded beads of high dimensional stability. The R411 represents the..