Polymer Property : Flexural Strength = 0.140 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 0.140 MPa
20.3 psi
Parallel to thickness
Zircar Ceramics AXHTM Alumina-Silica Insulation
ZIRCAR Alumina Silica Insulation Type AXL and Type AXHTM are inorganically bound insulation boards typified by their rigid outer surfaces and unbound interiors. They offer low thermal conductivity a..