Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 0.140 MPa | 20.3 psi | Parallel to thickness |
Zircar Ceramics AXHTM Alumina-Silica Insulation ZIRCAR Alumina Silica Insulation Type AXL and Type AXHTM are inorganically bound insulation boards typified by their rigid outer surfaces and unbound interiors. They offer low thermal conductivity a.. |