Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 99.88 MPa @Strain 4.40 %, Temperature 0.000 °C |
14490 psi @Strain 4.40 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 11C40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66 Minlon 11C40 NC010 is a 40% mineral reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |