Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 99.89 MPa @Strain 1.98 %, Temperature -20.0 °C |
14490 psi @Strain 1.98 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene.. |
|||
Tensile Stress | 99.89 MPa @Strain 1.98 %, Temperature -20.0 °C |
14490 psi @Strain 1.98 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5315HFS NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene.. |
|||
Tensile Stress | 99.91 MPa @Strain 1.83 %, Temperature 23.0 °C |
14490 psi @Strain 1.83 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Tensile Stress | 99.88 MPa @Strain 4.40 %, Temperature 0.000 °C |
14490 psi @Strain 4.40 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 11C40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66 Minlon 11C40 NC010 is a 40% mineral reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |