Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 96.5 MPa @Strain 12.0 %, Temperature -40.0 °C |
14000 psi @Strain 12.0 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider.. |
|||
Tensile Stress | 96.5 MPa @Strain 0.300 % |
14000 psi @Strain 0.300 % |
|
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |