Mechanical Properties Metric English Comments
Tensile Stress 65.6 MPa

@Strain 0.750 %,
Temperature 40.0 °C
9510 psi

@Strain 0.750 %,
Temperature 104 °F
ISO 527
DuPont Performance Polymers Crastin® SK608 BK509 PBT  (Unverified Data**)
Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 65.6 MPa

@Strain 0.750 %,
Temperature 40.0 °C
9510 psi

@Strain 0.750 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)  (Unverified Data**)
45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du..
Tensile Stress 65.6 MPa

@Strain 15.0 %,
Temperature 23.0 °C
9510 psi

@Strain 15.0 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AL NC010 an unreinforced high viscosity lubricated acetal homopolymer resin containing an advanced system of lub..
Tensile Stress 65.6 MPa

@Strain 15.0 %,
Temperature 23.0 °C
9510 psi

@Strain 15.0 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG100AL is a high viscosity lubricated acetal homopolymer resin containing ..