Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 93.8 MPa @Strain 5.11 %, Temperature -40.0 °C |
13600 psi @Strain 5.11 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It.. |
|||
Tensile Stress | 93.8 MPa @Strain 5.11 %, Temperature -40.0 °C |
13600 psi @Strain 5.11 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati.. |