Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 93.03 MPa @Strain 1.00 %, Temperature 23.0 °C |
13490 psi @Strain 1.00 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G35HSL BK262 is a 35% glass fiber reinforced heat stabilized black polyamide 6 resin for injection molding.Information provided by DuPont Per.. |