Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 63.0 MPa @Strain 3.80 %, Temperature 23.0 °C |
9140 psi @Strain 3.80 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Tensile Stress | 63.0 MPa @Strain 3.80 %, Temperature 23.0 °C |
9140 psi @Strain 3.80 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |
|||
Tensile Stress | 63.02 MPa @Strain 0.700 %, Temperature 23.0 °C |
9140 psi @Strain 0.700 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc.. |