Tensile Stress 6.29 MPa

@Strain 6.01 %,
Temperature 150 °C
912 psi

@Strain 6.01 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610  (Unverified Data**)
Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by..
Tensile Stress 6.29 MPa

@Strain 24.0 %,
Temperature 90.0 °C
912 psi

@Strain 24.0 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET  (Unverified Data**)
47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc..