Mechanical Properties Metric English Comments
Tensile Stress 9.67 MPa

@Strain 122.92 %,
Temperature 100 °C
1400 psi

@Strain 122.92 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 9.67 MPa

@Strain 0.530 %,
Temperature 120 °C
1400 psi

@Strain 0.530 %,
Temperature 248 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT  (Unverified Data**)
Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..