Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 9.19 MPa @Strain 70.25 %, Temperature 90.0 °C |
1330 psi @Strain 70.25 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |