Tensile Stress 9.14 MPa

@Strain 0.550 %,
Temperature 150 °C
1330 psi

@Strain 0.550 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen..
Tensile Stress 9.14 MPa

@Strain 221.82 %,
Temperature 100 °C
1330 psi

@Strain 221.82 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 9.14 MPa

@Strain 87.12 %,
Temperature 90.0 °C
1330 psi

@Strain 87.12 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 9.14 MPa

@Strain 87.12 %,
Temperature 90.0 °C
1330 psi

@Strain 87.12 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers