Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 9.07 MPa @Strain 94.05 %, Temperature 90.0 °C |
1320 psi @Strain 94.05 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |