Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 1320 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 9.10 MPa

@Strain 100 %
1320 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3896 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 9.09 MPa

@Strain 0.250 %,
Temperature 150 °C
1320 psi

@Strain 0.250 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7..
Tensile Stress 9.08 MPa

@Strain 5.00 %,
Temperature 23.0 °C
1320 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 9.07 MPa

@Strain 94.05 %,
Temperature 90.0 °C
1320 psi

@Strain 94.05 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 9.13 MPa

@Strain 3.60 %,
Temperature 150 °C
1320 psi

@Strain 3.60 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 9.12 MPa

@Strain 0.230 %,
Temperature 90.0 °C
1320 psi

@Strain 0.230 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66  (Unverified Data**)
40% Glass/Mineral Reinforced Polyamide 66 Zytel FE270038 is a 40% glass fiber/mineral reinforced heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.I..
Tensile Stress 9.09 MPa

@Strain 0.100 %,
Temperature 23.0 °C
1320 psi

@Strain 0.100 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc..
Tensile Stress 9.12 MPa

@Strain 30.0 %,
Temperature 80.0 °C
1320 psi

@Strain 30.0 %,
Temperature 176 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 9.12 MPa

@Strain 75.36 %,
Temperature 100 °C
1320 psi

@Strain 75.36 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..
Tensile Stress 9.12 MPa

@Strain 42.71 %,
Temperature 100 °C
1320 psi

@Strain 42.71 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me..
Tensile Stress 9.12 MPa

@Strain 79.75 %,
Temperature 120 °C
1320 psi

@Strain 79.75 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me..
Tensile Stress 9.13 MPa

@Strain 26.87 %,
Temperature 90.0 °C
1320 psi

@Strain 26.87 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me..
Tensile Stress 9.12 MPa

@Strain 42.71 %,
Temperature 100 °C
1320 psi

@Strain 42.71 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress 9.12 MPa

@Strain 79.75 %,
Temperature 120 °C
1320 psi

@Strain 79.75 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress 9.13 MPa

@Strain 26.87 %,
Temperature 90.0 °C
1320 psi

@Strain 26.87 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress 9.10 MPa

@Strain 100 %
1320 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 9.10 MPa

@Strain 100 %
1320 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G45D-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G45D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Copyright © lookpolymers.com All Rights Reserved