Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 9.04 MPa @Strain 56.83 %, Temperature 90.0 °C |
1310 psi @Strain 56.83 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.04 MPa @Strain 0.820 %, Temperature 150 °C |
1310 psi @Strain 0.820 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |