Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 58.81 MPa @Strain 1.32 %, Temperature 0.000 °C |
8530 psi @Strain 1.32 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G15L NC010 Nylon 6
(Unverified Data**) 15% Glass Reinforced Polyamide 6Zytel 73G15L NC010 is a 15% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 58.8 MPa @Strain 4.70 %, Temperature 23.0 °C |
8530 psi @Strain 4.70 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Tensile Stress | 58.8 MPa @Strain 2.52 %, Temperature 120 °C |
8530 psi @Strain 2.52 %, Temperature 248 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |