Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 84.8 MPa @Strain 3.10 %, Temperature 23.0 °C |
12300 psi @Strain 3.10 %, Temperature 73.4 °F |
ISO 11403-1 -2 |