Polymer Property : Tensile Stress = 12300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 84.7 MPa

@Strain 0.710 %,
Temperature 23.0 °C
12300 psi

@Strain 0.710 %,
Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Crastin® SK608 BK509 PBT  (Unverified Data**)
Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 85.0 MPa

@Strain 2.50 %,
Temperature 60.0 °C
12300 psi

@Strain 2.50 %,
Temperature 140 °F
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY
Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 85.0 MPa

@Strain 3.00 %,
Temperature 80.0 °C
12300 psi

@Strain 3.00 %,
Temperature 176 °F
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 85.0 MPa

@Strain 6.00 %,
Temperature 120 °C
12300 psi

@Strain 6.00 %,
Temperature 248 °F
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 85.0 MPa

@Strain 4.00 %,
Temperature 100 °C
12300 psi

@Strain 4.00 %,
Temperature 212 °F
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY
Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod..
Tensile Stress 85.0 MPa

@Strain 3.00 %
12300 psi

@Strain 3.00 %
Solvay TECHNYL® A 221 PA66, DRY
Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef..
Tensile Stress 85.0 MPa

@Strain 2.00 %
12300 psi

@Strain 2.00 %
Solvay TECHNYL® A 548B V15 PA66, 15% glass fiber, DRY
Description: TECHNYL® A 548B V15 is a copolyamide 6.6/6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits:..
Tensile Stress 85.0 MPa

@Strain 4.00 %,
Temperature 60.0 °C
12300 psi

@Strain 4.00 %,
Temperature 140 °F
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim..
Tensile Stress 85.0 MPa

@Strain 3.00 %
12300 psi

@Strain 3.00 %
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, Conditioned
Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers..
Tensile Stress 85.0 MPa

@Strain 1.00 %
12300 psi

@Strain 1.00 %
Solvay TECHNYLSTARâ„¢ S 218 V30 PA6, 30% glass filled, DRY
Description: TECHNYLSTARâ„¢ S 218 V30 is based on a patented high flow polyamide 6 resin (TechnylStar), heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is..
Tensile Stress 85.0 MPa

@Strain 1.00 %
12300 psi

@Strain 1.00 %
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc..
Tensile Stress 84.5 MPa

@Strain 18.2 %,
Temperature -20.0 °C
12300 psi

@Strain 18.2 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging..
Tensile Stress 84.5 MPa

@Strain 5.60 %,
Temperature -20.0 °C
12300 psi

@Strain 5.60 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper..
Tensile Stress 84.5 MPa

@Strain 5.60 %,
Temperature -20.0 °C
12300 psi

@Strain 5.60 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration ..
Tensile Stress 84.5 MPa

@Strain 3.50 %,
Temperature 23.0 °C
12300 psi

@Strain 3.50 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov..
Tensile Stress 84.9 MPa

@Strain 0.700 %,
Temperature -40.0 °C
12300 psi

@Strain 0.700 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
Tensile Stress 84.82 MPa

@Strain 1.46 %,
Temperature 23.0 °C
12300 psi

@Strain 1.46 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSLX BK357 is a 35% glass fiber reinforced heat stabilized black polyamide 66 for injection molding.Information provided by DuPont Perfor..
Tensile Stress 84.81 MPa

@Strain 1.25 %,
Temperature 90.0 °C
12300 psi

@Strain 1.25 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)  (Unverified Data**)
60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo..
Tensile Stress 84.8 MPa

@Strain 3.10 %,
Temperature 23.0 °C
12300 psi

@Strain 3.10 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers
Tensile Stress 84.6 MPa

@Strain 0.880 %,
Temperature 40.0 °C
12300 psi

@Strain 0.880 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66  (Unverified Data**)
40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P..
Tensile Stress 85.0 MPa

@Strain 4.00 %,
Temperature 40.0 °C
12300 psi

@Strain 4.00 %,
Temperature 104 °F
ISO 527
BASF Ultradur B 4300 G4 20% Glass Filled PBT
Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Tensile Stress 85.0 MPa

@Strain 4.00 %
12300 psi

@Strain 4.00 %
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY
Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit..