Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 57.71 MPa @Strain 1.53 %, Temperature 120 °C |
8370 psi @Strain 1.53 %, Temperature 248 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK609 NC010 PBT
(Unverified Data**) Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 57.7 MPa @Strain 2.30 %, Temperature -20.0 °C |
8370 psi @Strain 2.30 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Tensile Stress | 57.7 MPa @Strain 2.30 %, Temperature -20.0 °C |
8370 psi @Strain 2.30 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |
|||
Tensile Stress | 57.71 MPa @Strain 1.50 %, Temperature 120 °C |
8370 psi @Strain 1.50 %, Temperature 248 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA) Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance .. |
|||
Tensile Stress | 57.7 MPa @Strain 1.10 %, Temperature 0.000 °C |
8370 psi @Strain 1.10 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 57.7 MPa @Strain 0.720 %, Temperature 40.0 °C |
8370 psi @Strain 0.720 %, Temperature 104 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |