Mechanical Properties Metric English Comments
Tensile Stress 83.47 MPa

@Strain 3.88 %,
Temperature 40.0 °C
12110 psi

@Strain 3.88 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK602 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Polybutylene Terephthalate Crastin SK602 NC010 is a 15% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..
Tensile Stress 83.47 MPa

@Strain 3.85 %,
Temperature 90.0 °C
12110 psi

@Strain 3.85 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G35HSLRA4 BK267 is a 35% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection m..