Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 56.96 MPa @Strain 0.250 %, Temperature 40.0 °C |
8261 psi @Strain 0.250 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)
(Unverified Data**) 60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo.. |