Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 56.75 MPa @Strain 1.01 %, Temperature 90.0 °C |
8231 psi @Strain 1.01 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 95G50DH2 BK261 Nylon 6
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology only from DuPont providing exceptional Heat Resistanc.. |