Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 82.0 MPa @Strain 0.800 %, Temperature -40.0 °C |
11900 psi @Strain 0.800 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 82.0 MPa @Strain 3.00 %, Temperature 40.0 °C |
11900 psi @Strain 3.00 %, Temperature 104 °F |
ISO 527 |
BASF Ultradur B 4300 G4 20% Glass Filled PBT Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |