Polymer Property : Tensile Stress = 8190 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 56.5 MPa

@Strain 3.18 %,
Temperature 120 °C
8190 psi

@Strain 3.18 %,
Temperature 248 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66
Information provided by DuPont Performance Polymers