Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 56.5 MPa @Strain 3.18 %, Temperature 120 °C |
8190 psi @Strain 3.18 %, Temperature 248 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |