Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.44 MPa @Strain 0.400 %, Temperature 60.0 °C |
1220 psi @Strain 0.400 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66
(Unverified Data**) Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP.. |
|||
Tensile Stress | 8.44 MPa @Strain 0.180 %, Temperature 90.0 °C |
1220 psi @Strain 0.180 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610 30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Zytel RS 30G30L NC010 is a lubricated 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewabl.. |