Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.10 MPa @Strain 10.0 % |
1170 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® VT3108 TPC-ET Extrusion Grade, High Breathable, Drying of Material Required |
|||
Tensile Stress | 8.10 MPa @Strain 5.00 % |
1170 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc.. |