Mechanical Properties Metric English Comments
Tensile Stress 54.6 MPa

@Strain 12.6 %,
Temperature 23.0 °C
7920 psi

@Strain 12.6 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)  (Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri..