Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.28 MPa @Strain 39.03 %, Temperature 100 °C |
766 psi @Strain 39.03 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |