Mechanical Properties Metric English Comments
Tensile Stress 52.15 MPa

@Strain 7.00 %,
Temperature 180 °C
7564 psi

@Strain 7.00 %,
Temperature 356 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 54G35EF BK420 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced Toughened PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN54G35EF BK420 is a 35% glass reinforced toughened heat stabilized lubrica..
Tensile Stress 52.15 MPa

@Strain 1.35 %,
Temperature 90.0 °C
7564 psi

@Strain 1.35 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET)
20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol..