Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.08 MPa @Strain 0.300 %, Temperature 80.0 °C |
737 psi @Strain 0.300 %, Temperature 176 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |
|||
Tensile Stress | 5.08 MPa @Strain 108.54 %, Temperature 120 °C |
737 psi @Strain 108.54 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |