Polymer Property : Tensile Stress = 72.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 72.9 MPa

@Strain 1.50 %,
Temperature -20.0 °C
10600 psi

@Strain 1.50 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..
Tensile Stress 72.9 MPa

@Strain 7.00 %,
Temperature 23.0 °C
10600 psi

@Strain 7.00 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 311DP BK402 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP BK402 is a medium high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced..